This alpha-beta alloy is the workhorse alloy of the titanium industry. Titanium grade 5 has good tensile properties at ambient temperature and a useful creep resistance up to 300°C. Resistance to fatigue and crack propagation is excellent. Like most titanium alloys, Grade 5 has outstanding resistance to corrosion in most natural and many industrial process environments.

The ability to age harden this alloy makes it a good choice for such applications as springs and fasteners.

  • Applications

    Titanium Grade 5 is a pure alpha-beta titanium with aluminum as the alpha stabilizer and vanadium as the beta stabilizer. This alloy is primarily use for corrosion resistance and is the most widely used specification in all product forms. The alloy features very high strength, good corrosion resistance, excellent strength to weight ratio and high strength at cryogenic temperatures.

    Aerospace

      • Aircraft structural components (airframes, landing gear)
      • Jet engine parts (compressor blades, discs)
      • Spacecraft components requiring high strength and low weight
    Medical
      • Orthopedic implants (hip and knee replacements)
      • Dental implants
      • Surgical instruments
    Marine & Offshore
      • Propeller shafts and hardware exposed to seawater
      • Subsea equipment requiring high strength and corrosion resistance
    Automotive & Motorsport
      • High-performance engine components
      • Suspension parts
      • Racing applications where weight reduction is critical
    Industrial
      • High-pressure vessels and piping
      • Heat exchangers in corrosive environments
      • Components for chemical processing plants
    Defense
      • Armor plating
      • Military aircraft and naval components

     

  • Weldability

    Grade 5 alloy is easily welded in the annealed condition, or in the solution and partially aged condition, with aging being completed during the post weld heat treatment. Precautions must be taken to prevent oxygen, nitrogen, and hydrogen contamination. Fusion welding can be done in inert gas filled chambers, or using inert gas welding of the molten metal and the adjacent heated zones using a trailing shield.

    Spot, seam, and flash welding can be performed without resorting to protective atmospheres.

  • Chemical Composition

    Weight % Al V Fe N C O H Ti
    Min.  5,5  3,5
    Max.  6,8  4,5  0,25  0,05  0,08  0,2  0,015  BAL.
  • Mechanical Properties: Bar

    Yield strength Rp0.2,
    MPa
    Tensile strength Rm,
    MPa
    Elongation
    [%]
    Hardness
    [HRC]
    Impact, Charpy-V
    [J]
    Min. 828 897 10
    Max. 910 1000  18  36

Stocked products and dimensions

  • Round Bar

    DIA KG/M
    6 mm 0.14
    8 mm 0.23
    10 mm 0.4
    12 mm 0.6
    16 mm 1.
    20 mm 1.5
    25 mm 2.3
    30 mm 3.3
    32 mm 3.7
    35 mm 4.5
    38 mm 5.3
    40 mm 5.7
    43,7 mm 7.1
    45 mm 7.3
    48 mm 8.2
    50 mm 9.1
    55 mm 11
    60 mm 12.7
    63,5 mm 14.7
    70 mm 17.5
    76,2 mm 20.6
    80 mm 23.3
    90 mm 29.5
    100 mm 36.5
    115 mm 48.3
    120 mm 52.5
    130 mm 61.4
    140 mm 71.3
    150 mm 81.8
    180 mm 116
    200 mm 143
    225 mm 181
    255 mm 238